Contiguous hull structure: Production weld test

Edition and currency
eCFR text as of Sept. 29, 2026. The text is the edition Syfert holds; for a past event, check the version in force on that date.
Other sources
CURRENTeCFR text as of Sept. 29, 2026

If a portion of the contiguous hull structure is designed for a temperature colder than −34 °C (−30 °F) and is not part of the secondary barrier, each 100m (328 ft.) of full penetration butt welded joints in that portion of the contiguous hull structure must pass the following production weld tests in the position that the joint is welded:

(a) Bend tests under § 57.06-4 of this chapter.

(b) A Charpy V-notch toughness test under § 57.06-5 of this chapter on one set of 3 specimens alternating the notch location on successive tests between the center of the weld and the most critical location in the heat affected zone. 2

2 The most critical location in the heat affected zone of the weld is based on procedure qualification results, except austenitic stainless steel need have notches only in the center of the weld.

(c) If the contiguous hull structure does not pass the test under paragraph (b) of this section, the retest procedures under § 54.05-5(c) must be met.

Enactment and amendments

Syfert holds no separate history line for this section. Where this code prints a source or history note, it appears with the text, usually at the end.

Versions

Edition shown: eCFR text as of Sept. 29, 2026. Syfert holds no earlier or later version of this section.