Inspection and test of welds
(a) Visual inspection of welding must be conducted by an individual qualified by appropriate training and experience to ensure that:
(1) The welding is performed in accordance with the welding procedure; and
(2) The weld is acceptable under paragraph (c) of this section.
(b) The welds on a pipeline to be operated at a pressure that produces a hoop stress of 20 percent or more of SMYS must be nondestructively tested in accordance with § 192.243, except that welds that are visually inspected and approved by a qualified welding inspector need not be nondestructively tested if:
(1) The pipe has a nominal diameter of less than 6 inches (152 millimeters); or
(2) The pipeline is to be operated at a pressure that produces a hoop stress of less than 40 percent of SMYS and the welds are so limited in number that nondestructive testing is impractical.
(c) The acceptability of a weld that is nondestructively tested or visually inspected is determined according to the standards in section 9 or Appendix A of API Std 1104 (incorporated by reference, see § 192.7). Appendix A of API Std 1104 may not be used to accept cracks.
Syfert holds no separate history line for this section. Where this code prints a source or history note, it appears with the text, usually at the end.
Edition shown: eCFR text as of Sept. 29, 2026. Syfert holds no earlier or later version of this section.